Weld – Defects

By — February 10, 2011

We talk about type of welds & weld joints, the talk on welding will be incomplete if we don’t talk about weld defect!

Some weld defects are visible, some are visible with aide & some are invisible and need extra process to reveal them.

Before we go into process of different methods to see those defect, one must first know what are those defects?

Let me show you some defects & with their names

  • Spatter
  • Incomplete Fusion

  • Incomplete Penetration
  •  Overlap
  • Porosity 
  • Undercut 
  • Underfill 
Some are Visiable in Radiography!
Burn Thru
Cluster Porosity 
Excessive Reinforcement 
External Undercut 
Internal Undercut 
lack of penetration 
lack of fusion 
 Porosity
Suck Back 
Tungsten Inclusion 
in my next post, will discuss, i ndetail about the Methodology to see these cracks!

9 responses to “Weld – Defects”

  1. Natasha Drake, ndrake@dfbgroup.ca says:

    I'm writing my Level 1 visual inspection ticket this Wednesday and I thought your pictures on weld defects/faults were very helpful! Thanks so much for posting!

  2. Pertapa says:

    Thanks Pictures Information,

    Anang Yuniawan
    Indonesian

    All Best Regards

  3. Jerry gold says:

    I am preparing for my CWB visual Inspection and found your pictures helpful. Maybe some explanation and to the differences between some of the similar defects like Undercut, Underhill and Incomplete penetration will be of further help. But I am very grateful.

  4. Unknown says:

    Excellent Pictures, the radiographs next to the weld defects are excellent, thanks!

  5. Anonymous says:

    Plenty people are ruining this trade,they have no idea about how a rod burns or even know different polarity the CWB must stop this,when they come on site they only know undercut

  6. Anonymous says:

    I agree with Anonymous Friday, August 21, 2015

  7. This is how exactly welding is done. Thanks for sharing.

  8. Great,
    I observed how you explain Non-Destructive Testing, I'm working with a company for 30 years and we also use these common methods.